Key Features

Table unit for creep tests on different materials.

Flat specimens of lead and PE, 2 x 5 mm cross-section, 25 mm measured length.

Tensile stress range 5–25 N/mm2.

Position measurement gauge, 0–10 mm range, 0.01 mm resolution.

Tests above or below room temperature possible with a conditioning box.

Technical Specifications

SpecificationValue
Specimen materialLead, PE
Specimen cross-section2 x 5 mm
Measured length25 mm
Tensile stress range5–25 N/mm2
Position measurement range0–10 mm
Resolution0.01 mm

About This Product

A flat specimen is held under a set tensile stress while the position gauge tracks how its length changes over time. Testing both lead and PE specimens compares the creep behaviour of two different materials, and a conditioning box allows the same tests above or below room temperature. Colleges and TVET centres in Mongolia, Uganda, Fiji, Ghana and Slovenia can source the Creep Testing Machine from Educational Lab Equipments.

Frequently Asked Questions

Which specimens does the creep tester use?

Flat specimens made of lead and PE, with a 2 x 5 mm cross-section and a 25 mm measured length, loaded across a tensile stress range of 5–25 N/mm2.

Can creep be tested at other temperatures?

Yes. Experiments above or below room temperature are possible with a conditioning box.

How finely is elongation measured?

The position measurement gauge covers 0–10 mm with a resolution of 0.01 mm.

Related: Mechanics Training Models, Fatigue Testing Machine, Vibrations On Machine Foundations.

For a quotation on the Creep Testing Machine, contact Educational Lab Equipments.

   
Supply of Creep Testing Machine from to Finland, France, Tanzania, Thailand, Sri Lanka, Congo, Costa Rica, Ivory Coast, Croatia, Cuba, Cyprus, Czech Republic, Denmark, Djibouti, Dominica, Afghanistan, Albania, Algeria, Andorra, Angola, Antigua and Barbuda, Argentina, Armenia, Australia, Austria, Azerbaijan, Bahamas, Bahrain, Bangladesh, Barbados, United Arab Emirates (UAE, Dubai), United Kingdom (London), United States, Uruguay, Uzbekistan, Vanuatu, Belarus, Belgium, Belize, Benin, Bhutan, Bolivia, Bosnia and Herzegovina, Botswana, Brazil, Brunei, Bulgaria, Burkina Faso, Burma Myanmar, East Timor, Ecuador, Egypt, El Salvador, Equatorial Guinea, Eritrea, Estonia, Ethiopia (Addis Ababa), Fiji, Burundi, Cambodia, Cameroon, Canada, Cape Verde, Central African Republic, Chad, Chile, Colombia. Math Teaching Kit suppliers in Luxembourg, Macedonia, Madagascar, Malawi (Lilongwe), Malaysia (Kuala Lumpur), Maldives, Mali, Malta, Marshall Islands, Mauritania, Mexico, Micronesia, Moldova, Monaco, Mongolia, Montenegro, Morocco, Mozambique, Namibia, Comoros, Congo. Math Teaching Kit manufacturers in Dominican Republic, Gabon, Gambia, Georgia, Germany, Ghana, Greece, Grenada, Guatemala, Guinea, Guinea-Bissau, Guyana, Haiti, Honduras, Hungary, Iceland, Indonesia, Iran, Iraq, Niger, Nigeria (Abuja), Norway, Oman, Palau, Panama, Papua New Guinea, Paraguay, Peru, Philippines (Manila), Poland, Ireland, Israel, Italy, Jamaica, Japan, Jordan, Kazakhstan, Kenya (Nairobi), Kiribati, Korea, Kuwait, Kyrgyzstan, Laos, Latvia, Lebanon, Lesotho, Liberia, Liechtenstein, Lithuania, Mauritius, Nauru, Nepal, Netherlands, New Zealand, Nicaragua, Portugal, Qatar, Romania, Russia, Rwanda (Kigali). Math Teaching Kit exportets to Saint Kitts and Nevis, Saint Lucia, Saint Vincent and the Grenadines, Samoa, San Marino, Sao Tome and Principe, Saudi Arabia, Senegal, Serbia, Seychelles, Sierra Leone, Singapore, Slovakia, Slovenia, Solomon Islands, Somalia, South Africa, South Sudan, Spain, Sudan, Suriname, Swaziland, Sweden, Switzerland, Syria, Tajikistan, Togo, Tonga, Trinidad and Tobago, Tunisia, Turkey, Turkmenistan, Tuvalu, Uganda (Kampala), Ukraine, Venezuela, Vietnam, Yemen , Zambia (Lusaka), Zimbabwe

Office Address

Works: #449, HSIIDC, Industrial Area, Saha, Haryana,

[email protected]

Follow Us